Vitryne

Fabric & textile

The five physical fabric presets, their calibrated values and where they come from.

In short: five presets (cotton jersey, denim, poplin, fleece, wool suiting), each a set of physical values in SI units that the solver turns into stretch, shear and bending compliance. Use this page to see what a preset means, or to add one.

This page defines the five presets, their calibrated values, how they map to the XPBD solver, and the literature and measurement standards they come from.

The 5 presets at a glance

What each one is:

PresetCategoryWeight (g/m²)Thickness (mm)FrictionTarget strain (p99)
Cotton jerseyknit1500.450.30< 8% ✅
Denimwoven4200.850.42< 3% ✅
Poplin (shirting)woven1250.220.25< 3% ✅
Fleeceknit2802.200.38< 8% ✅
Wool suitingwoven2500.480.32< 3% ✅

How it stretches and bends (warp / weft where two numbers are given):

PresetStretch Y (N/m)Shear (N/m)Bending B (µN·m)
Cotton jersey14,000 / 9,0003,5006.0 / 4.0
Denim1,400,000 / 1,000,000400,000140 / 100
Poplin (shirting)1,100,000 / 800,000300,00018 / 12
Fleece28,000 / 18,0007,50075 / 55
Wool suiting850,000 / 650,000200,00032 / 24

All quantities use the Vitryne project format definitions (File format).


Physical units and solver mapping

1. Areal density (density, kg/m²)

  • Standard SI unit: kg/m² (100 g/m2=0.1 kg/m2100\text{ g/m}^2 = 0.1\text{ kg/m}^2).
  • In the engine: lumped vertex masses mim_i are accumulated from triangle rest areas AtA_t: mi=∑t∈triangles(i)13ρAtm_i = \sum_{t \in \text{triangles}(i)} \frac{1}{3} \rho A_t where ρ\rho is the areal density of the piece/cut the triangle belongs to.

2. Tensile and shear stiffness (stretch.warp, .weft, .shear, N/m)

  • Force per unit width per unit strain (ΔL/L0\Delta L / L_0), measured in N/m (or N/mm in some textile labs).
  • For an equilateral triangle lattice with spring stiffness kk, the equivalent continuum membrane has Young’s modulus Y=23kY = \frac{2}{\sqrt{3}} k and Poisson’s ratio ν=1/3\nu = 1/3.
  • In the engine, per-edge spring stiffness kk is derived from the mean membrane stiffness: k=32⋅Ywarp+Yweft2k = \frac{\sqrt{3}}{2} \cdot \frac{Y_{\text{warp}} + Y_{\text{weft}}}{2}
  • In XPBD, edge compliance is α=1/k\alpha = 1 / k (m/N\text{m/N}).

3. Bending rigidity (bending.warp, .weft, .bias, N·m)

  • Moment per unit width per unit curvature (M/κM / \kappa), in N⋅m\text{N}\cdot\text{m} (or μN⋅m=10−6 N⋅m\mu\text{N}\cdot\text{m} = 10^{-6}\text{ N}\cdot\text{m}).
  • In textile standards (KES-F), bending is typically reported in gf⋅cm2/cm\text{gf}\cdot\text{cm}^2/\text{cm}. The conversion factor is: 1 gf⋅cm2/cm=9.80665×10−7 N⋅m≈0.981 μN⋅m1\text{ gf}\cdot\text{cm}^2/\text{cm} = 9.80665 \times 10^{-7}\text{ N}\cdot\text{m} \approx 0.981\ \mu\text{N}\cdot\text{m}
  • In the engine, isometric bending constraints (Bergou et al. 2006, see Algorithms) use the mean bending rigidity B=12(Bwarp+Bweft)B = \frac{1}{2}(B_{\text{warp}} + B_{\text{weft}}) with XPBD compliance: αbend=Atri1+Atri26B\alpha_{\text{bend}} = \frac{A_{\text{tri1}} + A_{\text{tri2}}}{6 B}

4. Thickness (thickness, mm)

  • Compressed and uncompressed fabric thickness in mm.
  • Informational in v1; collision surface margins in the v1 engine are controlled by simulation settings (SimSettings.thickness), while fabric thickness provides the physical ground truth for rendering and export later.

5. Surface friction (friction, dimensionless)

  • Static/Coulomb friction coefficient against the avatar body.
  • Applied in the solver’s contact resolution step (SimSettings.friction).

Preset details and literature sources

1. Cotton Jersey

  • Construction: Single weft-knit, 100% combed cotton, 30s single yarn, typical everyday T-shirt.
  • Character: Very soft, stretchy, clinging, soft folds that follow the body contours closely.
  • Measurements:
    • Density: 0.15 kg/m20.15\text{ kg/m}^2 (150 g/m2150\text{ g/m}^2)
    • Thickness: 0.45 mm0.45\text{ mm}
    • Stretch: Ywarp=14,000 N/mY_{\text{warp}} = 14,000\text{ N/m}, Yweft=9,000 N/mY_{\text{weft}} = 9,000\text{ N/m}, G=3,500 N/mG = 3,500\text{ N/m}
    • Solver kk: ≈10,000 N/m\approx 10,000\text{ N/m} (Ymean=11,500 N/mY_{\text{mean}} = 11,500\text{ N/m})
    • Bending: Bwarp=6.0 μN⋅mB_{\text{warp}} = 6.0\ \mu\text{N}\cdot\text{m}, Bweft=4.0 μN⋅mB_{\text{weft}} = 4.0\ \mu\text{N}\cdot\text{m} (Bmean=5.0 μN⋅mB_{\text{mean}} = 5.0\ \mu\text{N}\cdot\text{m})
    • Friction: 0.300.30
  • Sources:
    • Kawabata (1980), The Standardization and Analysis of Hand Evaluation, 2nd ed., The Textile Machinery Society of Japan. Table 2.2 (knitted underwear fabrics).
    • Miguel, Tamstorf, Soto, Otaduy (2012), Data-Driven Estimation of Cloth Simulation Models, ACM Trans. Graph. 31(4), Table 1 (knit sample: low bending rigidity 4.2 μN⋅m4.2\ \mu\text{N}\cdot\text{m}, high weft extensibility).

2. Denim

  • Construction: Heavy 3/13/1 right-hand twill weave, 100% cotton, indigo warp / white weft, ≈12.5 oz/yd2\approx 12.5\text{ oz/yd}^2 (420 g/m2420\text{ g/m}^2), standard 5-pocket jeans.
  • Character: Stiff, heavy, robust. Resists bending; hangs away from the body in wide tubular folds; maintains crisp structural lines.
  • Measurements:
    • Density: 0.42 kg/m20.42\text{ kg/m}^2 (420 g/m2420\text{ g/m}^2)
    • Thickness: 0.85 mm0.85\text{ mm}
    • Stretch: Ywarp=1,400,000 N/mY_{\text{warp}} = 1,400,000\text{ N/m}, Yweft=1,000,000 N/mY_{\text{weft}} = 1,000,000\text{ N/m}, G=400,000 N/mG = 400,000\text{ N/m}
    • Solver kk: ≈1,039,000 N/m\approx 1,039,000\text{ N/m} (Ymean=1,200,000 N/mY_{\text{mean}} = 1,200,000\text{ N/m})
    • Bending: Bwarp=140 μN⋅mB_{\text{warp}} = 140\ \mu\text{N}\cdot\text{m}, Bweft=100 μN⋅mB_{\text{weft}} = 100\ \mu\text{N}\cdot\text{m} (Bmean=120 μN⋅mB_{\text{mean}} = 120\ \mu\text{N}\cdot\text{m})
    • Friction: 0.420.42 (coarser surface twill ribs increase drag against skin/avatar)
  • Sources:
    • Kawabata (1980), heavy workwear twills (B≈1.1 to 1.6 gf⋅cm2/cmB \approx 1.1\text{ to }1.6\text{ gf}\cdot\text{cm}^2/\text{cm}).
    • Breen, House, Wozny (1994), Predicting the Drape of Woven Cloth Using Interacting Particles, Table 1 (heavy cotton / denim bending parameters).
    • Clyde, Feng, Terzopoulos (2017), comparative woven benchmarks.

3. Poplin (Shirting)

  • Construction: Plain 1/11/1 weave with fine combed cotton yarns and high thread count (≈100×60\approx 100 \times 60), ≈3.7 oz/yd2\approx 3.7\text{ oz/yd}^2 (125 g/m2125\text{ g/m}^2).
  • Character: Crisp, lightweight, papery fine folds and sharp wrinkles, floats easily during movement.
  • Measurements:
    • Density: 0.125 kg/m20.125\text{ kg/m}^2 (125 g/m2125\text{ g/m}^2)
    • Thickness: 0.22 mm0.22\text{ mm}
    • Stretch: Ywarp=1,100,000 N/mY_{\text{warp}} = 1,100,000\text{ N/m}, Yweft=800,000 N/mY_{\text{weft}} = 800,000\text{ N/m}, G=300,000 N/mG = 300,000\text{ N/m}
    • Solver kk: ≈822,000 N/m\approx 822,000\text{ N/m} (Ymean=950,000 N/mY_{\text{mean}} = 950,000\text{ N/m})
    • Bending: Bwarp=18 μN⋅mB_{\text{warp}} = 18\ \mu\text{N}\cdot\text{m}, Bweft=12 μN⋅mB_{\text{weft}} = 12\ \mu\text{N}\cdot\text{m} (Bmean=15 μN⋅mB_{\text{mean}} = 15\ \mu\text{N}\cdot\text{m})
    • Friction: 0.250.25 (smooth combed cotton surface)
  • Sources:
    • Wang, O’Brien, Ramamoorthi (2011), Data-Driven Elastic Models for Cloth: Sub-Space Strain Limiting, ACM Trans. Graph. 30(4), Table 2 (cotton shirting poplin).
    • FAST-2 bending meter reference values for lightweight shirting (B≈0.12 to 0.20 μN⋅mB \approx 0.12\text{ to }0.20\ \mu\text{N}\cdot\text{m}).

4. Fleece

  • Construction: Double-faced brushed polyester knit (sweatshirt fleece / microfleece), ≈280 g/m2\approx 280\text{ g/m}^2.
  • Character: Lofty, thick, plush. Rounded, puffy folds; soft elastic compliance; high air drag and bulk.
  • Measurements:
    • Density: 0.28 kg/m20.28\text{ kg/m}^2 (280 g/m2280\text{ g/m}^2)
    • Thickness: 2.20 mm2.20\text{ mm}
    • Stretch: Ywarp=28,000 N/mY_{\text{warp}} = 28,000\text{ N/m}, Yweft=18,000 N/mY_{\text{weft}} = 18,000\text{ N/m}, G=7,500 N/mG = 7,500\text{ N/m}
    • Solver kk: ≈20,000 N/m\approx 20,000\text{ N/m} (Ymean=23,000 N/mY_{\text{mean}} = 23,000\text{ N/m})
    • Bending: Bwarp=75 μN⋅mB_{\text{warp}} = 75\ \mu\text{N}\cdot\text{m}, Bweft=55 μN⋅mB_{\text{weft}} = 55\ \mu\text{N}\cdot\text{m} (Bmean=65 μN⋅mB_{\text{mean}} = 65\ \mu\text{N}\cdot\text{m})
    • Friction: 0.380.38 (fibrous brushed pile)
  • Sources:
    • Kawabata (1980), winter outerwear knits and pile fabrics.
    • FAST-1 compression and thickness standards for brushed fleece goods (h>2.0 mmh > 2.0\text{ mm}).

5. Wool Suiting

  • Construction: Worsted wool 2/22/2 twill, high-twist 2-ply yarn, ≈7.5 oz/yd2\approx 7.5\text{ oz/yd}^2 (250 g/m2250\text{ g/m}^2), tailored jacket and trouser cloth.
  • Character: Resilient, tailored roll, elegant fluid drape with clean creases; does not collapse limp or buckle abruptly.
  • Measurements:
    • Density: 0.25 kg/m20.25\text{ kg/m}^2 (250 g/m2250\text{ g/m}^2)
    • Thickness: 0.48 mm0.48\text{ mm}
    • Stretch: Ywarp=850,000 N/mY_{\text{warp}} = 850,000\text{ N/m}, Yweft=650,000 N/mY_{\text{weft}} = 650,000\text{ N/m}, G=200,000 N/mG = 200,000\text{ N/m}
    • Solver kk: ≈650,000 N/m\approx 650,000\text{ N/m} (Ymean=750,000 N/mY_{\text{mean}} = 750,000\text{ N/m})
    • Bending: Bwarp=32 μN⋅mB_{\text{warp}} = 32\ \mu\text{N}\cdot\text{m}, Bweft=24 μN⋅mB_{\text{weft}} = 24\ \mu\text{N}\cdot\text{m} (Bmean=28 μN⋅mB_{\text{mean}} = 28\ \mu\text{N}\cdot\text{m})
    • Friction: 0.320.32
  • Sources:
    • Kawabata (1980), Table 2.1 (men’s worsted suiting fabrics, B≈0.25 to 0.35 gf⋅cm2/cmB \approx 0.25\text{ to }0.35\text{ gf}\cdot\text{cm}^2/\text{cm}).
    • Minami, Minami, Maekawa (2002), Fabric Drape and Physical Properties, J. Textile Eng. 48(6), worsted suiting drape coefficients.